For all the experiments mobile phones were disassembled in order to remove PCBs Then these were cut into small pieces of up to 5 mm Samples of cut PCBs were ground in a hammer mill in order to reduce their size to 1 mm After that roasting at 0 72 atm 21 oxygen and 850°C was applied to PCB samples for plastic removal }